The high temperature properties, coke reactivity index (CRI) and coke strength after reaction (CSR) are improved with longer carbonization time.
随着结焦时间的延长,焦炭的热态性能,即焦炭反应性(CRI)和反应后强度(CSR),均得到提高。
The experimental results showed that coke reactivity is increased with lime stone addition and reduced with pitch addition, but the coke strength after reaction is increased.
实验结果表明,加入石灰石后焦炭的反应性显著升高,加入沥青后焦炭的反应性降低,反应后强度提高。
Under the same temperature, Strength of coke increases after the reaction and coke fines decreases as the amount of UPC being injected into coke layer increases.
同一温度条件下,随着焦炭层喷吹UPC量的增加,气化反应后焦炭的强度提高,粉末量减少。