The main characteristics of edge cracking and scab have been analyzed.
分析了边裂、翘皮的主要形态特征;
The mechanism and cause of edge cracking defect of hot-rolled strip in Kunming Iron & Steel co.
对昆钢热轧板卷边裂缺陷机理及成因进行了研究分析,提出了相应的预防控制措施,取得了较好的效果。
Structure testing in low magnificution, chemical composition analysis and microstructure examination were used to analyze the edge cracking of strip steel coil.
采用低倍组织试验、化学成分分析及金相检验等方法,对出现边裂的带钢卷进行了解剖分析。