... 镍基高温合金 Nickel-based Super Alloy 钴基高温合金 Cobalt-base superalloy 耐蚀合金 Corrosion resistand Alloy ...
基于10个网页-相关网页
DZ40M (a directionally solidified cobalt-base superalloy) has been used to fabricate turbine vanes at a working temperature below 1050 oC.
DZ40M合金是一种定向凝固钴基高温合金,适用于工作温度在1050 oC以下的导向叶片。
参考来源 - DZ40M高温合金的再结晶及其对合金力学性能的影响·2,447,543篇论文数据,部分数据来源于NoteExpress
This article studies a new type cobalt-base superalloy GH941 including its composition, structures and mechanical properties.
本文研究了新型钴基高温合金GH941的成分、组织及性能。
The effect of aging treatment on the tensile strength, elongation, hardness and microstructure of a cobalt base superalloy used for pistons rings was investigated in this paper.
本文研究了不同热处理时效温度和时效时间对一种活塞环用钴基高温合金的抗拉强度、延伸率、硬度及组织的影响。
GH543 cobalt-free nickel base superalloy is finally selected from the final 12 compositions extracted through theoretical analysis.
无钴镍基高温合金GH 543即是从理论分析的最终的12种成分中选择出来的。
应用推荐