The hardening case depth and hardness curve can be changed by adjusting heating time, heating power and cooling speed during induction hardening.
在感应淬火中,通过改变加热时间、加热功率和冷却速度可以改变淬硬层深度和硬度梯度。
Nitriding develops extreme hardness in the surface of steel. This hardness ranges from 900 to 1,100 Brinell, which is considerably higher than that obtained by ordinary case hardening.
渗氮在钢表面获得远远超出正常标准的硬度。其硬度范围为900到1,100布氏硬度,这远高于普通表面硬化所获得的硬度。
This hardness ranges from 900 to 1,100 Brinell, which is considerably higher than that obtained by ordinary case hardening.
其硬度范围为900 到1,100 布氏硬度,这远高于普通表面硬化所获得的硬度。