实验结果表明,镀膜后其单面剩余反射率由未镀膜时的2.5%减少到1.2%,并能承受湿热和雨淋测试。
The experimental results show that after coating the single residual reflectance was reduced from 2.5% to 1.2% and could withstand the muggy and rain testing.
实验结果表明,镀膜后其单面剩余反射率由未镀膜时的2.5%减少到1.2%,并能承受湿热和雨淋测试。
The experimental results show that after coating the single residual reflectance was reduced from 2.5% to 1.2% and could withstand the muggy and rain testing.