电阻点焊是铝合金薄板主要连接技术之一。
Resistance spot welding is one of the main connection technology for aluminum alloy thin sheet.
对两种形式的温差拉伸控制铝合金薄板焊接残余变形的效果和规律进行了研究。
The effects of distortion control in welding thin aluminum alloy plates by two kinds of thermal tensioning were investigated.
利用高功率CO2激光器,对5083型号的铝合金薄板进行了焊接试验研究。
Laser welding of 5083 aluminum alloys with high power CO2 laser is experimental studied in this paper.
研究了随焊激冷减小铝合金薄板焊接变形的效果及夹具的散热条件对该效果的影响。
Effectiveness of reducing welding distortion by trailing intensive cooling and the influence of heat - dissipating condition of the fixture on such effectiveness were studied.
应用高效的气体保护熔化极电弧焊焊接铝合金薄板时,容易出现熔池下塌、烧穿等焊接缺陷。
Welding defects such as collapse of molten pool, burning through, would like to happen in the high efficient gas shielded metal arc welding.
对温差拉伸和随焊激冷配合使用控制铝合金薄板焊接变形的联合工艺进行了数值模拟和试验研究。
The technique using thermal tensioning and trailing intense cooling simultaneously to reduce welding distortion was investigated by both numerical simulation and experiments.
对喷成形技术是结合铝合金薄板件的特点,在喷丸成形和强化工艺基础上,提出的一种边缘工艺技术。
Based on the characteristic of thin aluminium skin, shot peening and peening forming, peening forming by double face is a new mixed process.
本文对机械闹钟夹板以铝合金薄板代替铜带之后的一次冲多个小孔的工艺及模具结构进行了分析、探讨。
This article analyzes and discusses the technology and model tool structure of aluminium-alloy thin-plate instead of brass band to punch several small hole one time.
对ZL114A铝合金薄板采用激光填丝焊接,通过三种不同成分的铝合金焊丝,向焊缝中添加合金元素。
ZL114A aluminum alloy sheet was tested by laser filler wire welding . Through the three different alloy compositions of aluminum alloy welding wire, to add different alloy element to the weld.
表面淬火钢,铜、铝合金薄板,带钢,硬质合金钢,镀锌,镀铬,镀锡,材料表面热处理和化学表面处理的各种金属材料。
Surface hardened steel, copper, aluminum alloy sheet, hard alloy steel, zinc layers, chrome layers, tin layers, surface heat treating and chemical treating materials, etc.
适用范围表面淬火钢,铜、铝合金薄板,带钢,硬质合金钢,镀锌,镀铬,镀锡,材料表面热处理和化学表面处理的各种金属材料。
Usage Range: Surface hardened steel, copper, aluminum alloy thin sheet, hard alloy steel, zinc layers, chrome layers, tin layers, surface hardened treating and chemical treating materials, etc.
铜合金铸件,薄板、不锈钢带、铝合金铸件除锈、除氧化皮及表面强化。
Derusting, oxide skin removing and surface hardening for copper castings, sheet metal, stainless steel strips, aluminum castings.
脉冲电流幅值和EP半波时间对铝合金表面氧化膜的清理有重要影响,在焊接薄板铝合金时应采用较低的脉冲频率。
The pulsed current peak value and EP time have a important effect on removal of the surface oxide, the lower frequency should be adopted for thin sheet of aluminium alloy.
利用温度与变形实时测量系统,对铝合金5a12薄板氩弧焊接动态角变形过程进行了试验研究,探讨通过特征值来描述角变形动态行为。
The characteristics of dynamic welding angular distortions of aluminum alloy 5a12 with tig welding are investigated by self-made welding dynamic temperature and distortion measuring system.
添粉和不添粉的5A02和5A06铝合金拼焊板的横向拉伸试件均断裂于薄板母材,证明焊缝的强度合格。
The longitudinal tension PM specimen of Tailor Welded Blanks of 5A02 and 5A06 were all fractured on the thinner base metal, which indicated that welds were eligibility.
添粉和不添粉的5A02和5A06铝合金拼焊板的横向拉伸试件均断裂于薄板母材,证明焊缝的强度合格。
The longitudinal tension PM specimen of Tailor Welded Blanks of 5A02 and 5A06 were all fractured on the thinner base metal, which indicated that welds were eligibility.