金精矿可直接作为产品,钨粗精矿可返回现场流程作进一步的处理。
The gold concentrate can be used as products directly and Tungsten coarse concentrate should be sent to the on-site process for retreatment.
通过对选铁尾矿中回收铁精矿的工艺考查、分析,进行了粗精矿再磨工艺的试验。
The experimental study on the re-grinding of primary concentrate has been conducted through the investigation and analysis on the process to recover iron concentrate from tailings of ore dressing.
本文论述采用亚硫酸盐作抑制剂,对黑钨粗精矿精选枱浮钼、铜、铋硫化矿浮选分离的研究。
The flotation separation of molybdemun, copper and bismuth sulfides minerals, which are obtained by table flotation of wolframite primary concentrates, is studied using sulphites as depressants.
对化学组成和粒度不同的红柱石精矿和粗精矿在不同温度下的莫来石化行为进行了X射线分析。
Mullitization of concentrated andalusite in different chemical composition and different grain size has been determined at different temperatures by mcans of X-ray analysis.
试验研究依据矿物特性,采用铅锌等可浮,粗精矿再磨措施,有效地解决了铜铅锌矿物分离问题。
According to the minerals characteristic, the experiment developed con? flotationable flotation flewsheet and Pb, Zn mixed concentrate regrinded to successfully separate Pb and Zn.
本发明给出了一个用有着特殊结构的气体鼓泡流体床,对石棉粗精矿或含石棉产物进行精选的方法。
This invention relates to a method to sort coarse clean asbestos ore of asbestos-containing products with a gas-bubbling fluidized bed having a special structure.
磁选柱的分选特点是把磁铁矿连生体颗粒有效地从磁铁矿粗精矿中分选出来,从而获得高品位的铁精矿。
The separation characteristic of Cloumn magnetic separator is that the particles of "locked" mineral are separated efficiently from low grade magnetic mineral. Thus producing...
探索大石河选厂在生产流程的基础上,应用螺旋溜槽,获取粗磨后最终精矿的可能性。
Based on the processing flow of Dashihe separation mill, using spiral sluice, the possibility of obtaining final concentrate under coarse primary grinding is searched for.
对于富矿的选别,采用粗磨跳汰—摇床的技术方案,得到的锰精矿品位为40.41%,回收率为70.92%的选别指标。
A technical scheme of grinding-waving bed to be sifted out is adopted and the fined ore grade can reach 40.41%. The rate of recovery is 70.92% in choosing target.
对于富矿的选别,采用粗磨跳汰—摇床的技术方案,得到的锰精矿品位为40.41%,回收率为70.92%的选别指标。