• 砂眼打光可以达到镜面效果

    Trachoma. Lighting can be achieved after the mirror effect.

    youdao

  • 熔模铸造砂眼缺陷产生因素进行了分析

    Carried on the analysis to the lost wax casting craft sand hole defect creation factor.

    youdao

  • 后天性睫毛原因常见砂眼所引起的。

    Acquired inverted eyelashes reasons, the most common is caused by Shayan.

    youdao

  • 介绍粘合剂修补铸件砂眼、气孔缺陷方法

    The method by using the adhesive for repairing casting defects such as sand holes and air holes has been described in this article.

    youdao

  • 砂眼可以接受暴露金属的电镀附著不可接受。

    Blisters are not acceptable. Improper adhesion which exposes bare metal is not acceptable.

    youdao

  • 表面瑕疵例如碎片,烧痕,渣,砂眼应用磨光机打磨

    Surface imperfections, such as slivers, scabs, burrs, weld splatter, and gouges, shall be removed by grinding.

    youdao

  • 因为砂眼造成眼睑板结膜结疤进而导致眼睑内翻睫毛

    Shayan because the board will cause the eyelids and conjunctiva scarring, thus leading to eyelid inversion and inverted eyelashes.

    youdao

  • 高速离心铸造组织致密,砂眼夹渣表面光滑厚均匀

    Centrifugal casting, compact structure, free from pinhole porosity and slag, smooth surface and even wall thickness.

    youdao

  • ,易加工,但抗裂性较受力灰铸铁加工砂眼补焊。

    Copper nickel, good machinability bad crack resistance. Repair welding of shole gray cast iron machined surface subject to no load.

    youdao

  • ,易加工,但裂性较受力灰铸铁加工砂眼补焊。

    Copper nickel good machinability and bad crack resistance. Repair welding of sand hole and gray cast iron machined surface subject to no load.

    youdao

  • ,易加工,但抗性较受力灰铸铁加工砂眼补焊。

    Copper nickel, good machinability and bad crack resistance. Repair welding of sand hole and gray cast iron machined surface subject to no load.

    youdao

  • 铸铁件含碳量结构疏松、表面大量砂眼缺陷,增加电镀难度。

    High carbon content of iron castings and defects of incompact structure and a great deal of sand holes on the surface of iron castings make it difficult for electroplating.

    youdao

  • 结果表明:铸件表面光洁砂眼、气孔等缺陷,铸件合格率高于90%;

    The defects of sand-slag and gas-hole are absent in the water-cooling-sprayer whose surface is clean and qualified rate is more than 90%.

    youdao

  • 铸造技术不完善、合金原料中的杂质致使水龙头零件表面疏松,并有大量砂眼

    The defects of casting technology and the impurities in copper alloy material cause roughness of faucet surface with large amounts of sand holes.

    youdao

  • 所有分界面能反射声波到达某个程度包括龟裂、内容砂眼分布范围其它裂痕

    All interfaces will reflect or scatter waves to some degree. This includes cracks, inclusions, grain boundaries and other discontinuities.

    youdao

  • 其中新添的珍珠、龙睛水泡蛋球、蛋品种

    Updates to the eye in which a dragon ball, pearl dragon eyes, dragon eyes Bubble eye, cinnabar eyes, silver egg, blue egg balls, egg balls back, egg kind of turned gill and other varieties.

    youdao

  • 其中珍珠、龙睛水泡、朱砂眼蛋球、蛋球、蛋种品种。

    One of the new dragon ball, pearl dragon eye eye, eye, eye blisters, t., silver, blue eggs, eggs, a ball back eggs over the gills, etc.

    youdao

  • - “黑盒子” -只是一个提示自然光线通过纳入地方虹膜外部格局喷混凝土

    Gallery Three – the "black box" – has only a hint of natural light, integrated into and through the iris of the sandblasted eye pattern on the exterior cast in place concrete walls.

    youdao

  • 选择仿大理石线条时,应对线条表面是否平整棱角有无缺陷,有无裂纹划痕,有无砂眼色调是否纯正方面进行筛选

    In the choice of imitation marble lines, but also deal with the line surface is smooth, edges have no defect, no cracks, scratches, or trachoma, whether pure color screen areas.

    youdao

  • 选择仿大理石线条时,应对线条表面是否平整棱角有无缺陷,有无裂纹划痕,有无砂眼色调是否纯正方面进行筛选

    In the choice of imitation marble lines, but also deal with the line surface is smooth, edges have no defect, no cracks, scratches, or trachoma, whether pure color screen areas.

    youdao