• 硫化锌精矿焙烧中性含有等有价元素,常规低酸高酸浸出流程锗的直收率低。

    Neutral leaching residue of roasted zinc concentrate often contains germanium which is poorly recovered in conventional two-stage leaching.

    youdao

  • 重点探讨低温温度时间,高温焙烧温度及时间浸出率的影响。

    The effects of acid to materials ratio, roasting temperature and time in low roasting action and high roasting action on the Ni and Co leaching were investigation, respectively.

    youdao

  • 浸出滤液二氧化硫烟道气还原,还原液经冷冻结晶过滤精制后可得纯度较高精白砷

    High purity arsenic trioxid was obtained from the 2nd stage filtrate by reduction with SO2 flue gas, freeze crystallization, water dissolving, filtering and refining.

    youdao

  • 浸出滤液二氧化硫烟道气还原,还原液经冷冻结晶过滤精制后可得纯度较高精白砷

    High purity arsenic trioxid was obtained from the 2nd stage filtrate by reduction with SO2 flue gas, freeze crystallization, water dissolving, filtering and refining.