随着温度的升高其平衡含水率下降。
As the temperature increases the equilibrium moisture content decreased.
动态平衡含水率与乾燥热风温度,谷物之关系可加以建立。
The relationship among Mde, drying air, and grain properties could be established.
资料表明,木材经热处理改性后,尺寸稳定性增强、平衡含水率降低,且耐候性及抗生物降解能力增强。
The data shows that after heat-treatment, the dimensional stability of lumber is greatly improved, the EMC is reduced, and the weather resistant properties and durability to bio.
炭化木的质量指标主要有木材平衡含水率比未处理材低3%左右,干缩率小于5%,优于柚木的7%。
The main quality indexes of coking wood has wood balance moisture content than unprocessed materials low around 3%, dry shrinkage rate less than 5%, superior teak 7%.
根据某算例,采用极限平衡分析方法,讨论了土体的初始体积含水率、降雨的强度、降雨时间对边坡稳定性的影响程度。
The paper according to a calculating example to use limiting equilibrium analysis discussed soil mass original bulk water content rainfall intensity rainfall time impact extent to slope stability.
在微波真空干燥过程中,就整个板材而言,热扩散效应对木材中水分迁移的影响不大,但在局部的有限范围内,它对自动平衡木材内含水率具有显著的作用。
During the drying process of MV, for the whole board, the effect of thermal diffusion on moisture movement is not significant, but it can cause a leveling of moisture profile in a local range of wood.
干燥后板材的含水率在材堆内分布均匀,在板材厚度方向分布有一定差异,平衡后可以使用;
However, a moisture content gradient occurred along the thickness direction but could be (balanced) after about a week.
干燥后板材的含水率在材堆内分布均匀,在板材厚度方向分布有一定差异,平衡后可以使用;
However, a moisture content gradient occurred along the thickness direction but could be (balanced) after about a week.