• This article mainly reasearched that light alkali substituting heavy alkali and 10% silica sand ultra-fine dust were used in the float glass batch by the method of adding special cementing agent.

    通过浮法玻璃配合加入特殊黏结取代传统配合料加水,可以将配合料中换成碱,可利用10%的硅质超细粉原料

    youdao

  • Using nepheline syenite as a substitute for feldspar, the batch mixtures were prepared on a composition of float glass and are melted into glasses.

    霞石正长岩取代长石,按照浮法玻璃成份制备配合料熔制玻璃。

    youdao

  • Using nepheline syenite as a substitute for feldspar, the batch mixtures were prepared on a composition of float glass and are melted into glasses.

    霞石正长岩取代长石,按照浮法玻璃成份制备配合料熔制玻璃。