目的:了解电解质和电压因素对氧化膜成分、形态和稳定性能的影响。
Objective: To know the effects of electrolyte and voltage on the property of anodic oxide films.
结论蜂王浆与蜂花粉复合剂可通过减少机体ROS生成,增加线粒体膜稳定性,缓解老龄大鼠机体氧化应激状态。
Conclusions The compound of royal jelly and bee pollen could relieve oxidative stress of aged rats through decreasing production of ROS and increasing stability of MMP.
采用电化学氧化技术在玻碳电极(GCE)表面制备了稳定的赖氨酸单层膜。
A stable Lysine monolayer was obtained on the surface of glassy carbon electrode (GCE) by means of electrochemical oxidation method.
铝质材料在空气中是极不稳定的,容易形成用肉眼难以识别的氧化膜。
Aluminum material in air is very unstable easy to form with the naked eye, it is difficult to identify the oxide film.
结果还表明PS A是一种具有耐热、抗氧化和化学稳定性的合成膜材料。
In addition, the results also show that PSA ultrafiltration membrane is one with good thermal, oxidative and chemical stability.
焊点中存在的主要缺陷是气孔,表面下塌,热裂纹,其中气孔主要为氧化膜气孔和匙孔不稳定形成的气孔。
The main defects of laser spot welding of aluminum are crater, hot crack and porosity which created by oxide film and keyhole instability,.
但天然磷脂作为脂质体膜材,由于其寿命短、易被氧化、稳定性差等缺点,应用受到限制。
The usage of natural phospholipids was limited for the disadvantages of short life, frangibility to oxidation and less stableness.
研究了憎水基团的添加量对溶胶体系的稳定性和对二氧化硅膜润湿性以及水汽稳定性的影响。
The influences of hydrophobic group content on the stability of the silica sols and the surface wettability and vapour stability of the silica membranes were investigated.
对于空气氧化膜,电化学反应速度逐步变慢,直至达到相应于稳定钝态的恒定值,同时电位向正移动,表明膜中的微裂纹不断得到修补。
With air-formed films the faradaic processes decreased progressively to a constant rate consistent with the increase in potential, indicating the healing of surface flaws.
并探讨了嫁接反应中影响单分子膜特性的某些因素和单分子膜的稳定性及其对硅表面氧化的钝化作用。
Some factors influencing the properties of the monolayers, their stability and passivation towards oxidation of silicon surface were examined.
对氧化膜的组分和稳定性,以及MOS结构的C—V特性进行了实际测量和理论分析。
The stability and composition of oxidic film and the C-V characteristics of MOS structure have also been tested and analysed theoretically in this paper.
提供了该厚膜与氢和一氧化碳的反应数据,它的电导率和化学稳定性均好。
Data on the hydrogen and carbon monoxide responses of thick film is reported. Both the electronical conductivity and chemical stability of the thick-film are good enough.
共混膜具有较好的热稳定性、氧化稳定性和力学性能。
Besides, the thermal stability, mechanical strength and oxidation stability were also good enough for demand of AAEMFC.
结果表明,6 -MHA在金电极表面能够形成一层稳定的自组装膜,并对叶绿素的氧化还原过程具有明显的催化作用。
The results show that 6 MHA can form stable SAM on gold electrode, and this 6 MHA SAM electrode has obvious catalysis for the REDOX reaction of chlorophylls.
膜有稳定的氧化还原电流峰,电位漂移小,重现性好,适合于制成新型参比电极。
POAP-Fe(CN)3-6 film has a stable redox current peak, a small potential drift and a good repeatability, and it can be used as a new model reference electrode.
膜有稳定的氧化还原电流峰,电位漂移小,重现性好,适合于制成新型参比电极。
POAP-Fe(CN)3-6 film has a stable redox current peak, a small potential drift and a good repeatability, and it can be used as a new model reference electrode.
应用推荐