马佘乐打电话给中国的模具厂:「CAE指出:必须 在开口采用薄膜浇口,该浇口沿原开口长边的厚度 是0.5mm,沿原开口短边的厚度是1.5mm。」
Marthaler called the Chinese toolmaker:"CAE indicates that a diaphragm gate at 0.5mm deep on the long side and 1.5mm deep on the short side should be used."
马佘乐打电话给中国的模具厂:「CAE指出:必须 在开口采用薄膜浇口,该浇口沿原开口长边的厚度 是0.5mm,沿原开口短边的厚度是1.5mm。」
Marthaler called the Chinese toolmaker:"CAE indicates that a diaphragm gate at 0.5mm deep on the long side and 1.5mm deep on the short side should be used."