对蠕变内应力的测试方法进行研究。
In this paper, measuring method of creep internal stress are studied.
退火也释放了先前在金属中的内应力。
Annealing also relieves internal stresses previously set up in the metal.
您将获得在几分钟内应力结果和变形。
You will get stress results and deformations within a few minutes.
去除内应力,如用冲压、完全或焊接成型的工件。
To remove internal stress such as those produced by drawing, bending, or welding.
从内应力成因入手,分析了内应力对钻头性能的影响。
From source of it, analyses inner-stress affection to bit performance.
倒置法的依据是在模型倒置时测定模型内应力分布的变化。
This method depends on determining the change in stress distribution within the model when it is turned upside down.
研究表明:应力(包括内应力)明显地影响点阵的稳定性。
The results show that the stress has strong effects on the lattice instability.
轴承零件在淬火冷却过程中因内应力所形成的裂纹称淬火裂纹。
Bearing parts in the process of hardening cooling by internal stress due to the formation of quenching cracks crack said.
当纱线被加捻的时候,在捻度的方向上也会相应地形成内应力。
As the yarn is twisted, internal forces are built up in the direction of the twist.
热轧带钢局部高点对冷轧带钢板厚和内应力分布具有重要影响。
The hot strip local high points have very important influence on the internal stress distribution and thickness of cold strip.
电镀后用加热法除内应力或电镀时与1%的铅共沉积可避免这一特性。
After plating with heating except with 1% of the internal stress or plating of sedimentary can avoid this lead a characteristics.
从理论上计算了非晶态薄带中不同区域的内应力场和应力磁各向导性。
The internal stress fields and the stress-magnetic anisotropies in different regions of the amorphous ribbon were calculated theoretically.
从钢管壁上任意一点的环向应力入手,分析了长输管道焊缝的内应力。
Internal stress of welds seam for long distance pipeline is analyzed starting with any point of circumferential stress on pipe wall.
侵彻时的应力状态与压入法测硬度相似,靶内应力状态为三向压应力。
The penetration process is similar to Vickers hardness test, it is triaxial compressive stress condition in the target.
激光成形技术是以激光为热源加热金属板料,依靠内应力使板料弯曲成形。
Laser forming is a flexible forming process that forms sheet metal by means of stresses induced by the laser beam.
介绍了渗碳淬火零件热处理畸变的原因,分析了热处理内应力的形成过程。
The present paper analyzed the reasons of heat treatment distortion of carburizing and hardening components and the formation process of the internal stress.
淬火过程中的快速冷却在工件内部产生的内应力是导致淬火变形的根本原因。
The stress produced by quick cooling inside workpiece during quenching treatment is the main reason of quenching deformation.
内应力的分布,对材料宏观力学性能如强度和断裂韧性,都将产生较大的影响。
The distribution of internal stress has large influence on mechanical properties of materials such ay strength and fracture toughness.
内应力是造成高铬白口铸铁磨球在生产和服役过程中出现变异和失效的主要原因。
Variation and failure of the grinding ball of high chromium white cast iron during production and service are mainly caused by the internal stress.
湿整过程中,织物将释放在织造过程中产生的内应力,还织物以羊毛的自然特性。
After wet finishing, the fabric will release its inner stress that produced on the process of weaving and regain its natural characteristics as wool.
方法:用二维有限元法分析阻萌力减少前后下第一磨牙牙周组织内应力分布的变化。
Metbods: a two dimensional finite element model was built up to analyse the stress within the periodontal tissue of the first molar, with a reduced tooth eruption-resistant force.
本文研究了一种制备高硬度、低内应力、厚度高且热稳定性良好的非晶碳薄膜的方法。
We have developed a new process for building up thick and stable amorphous carbon films with high hardness and low internal stress.
传统工艺条件下,高铬铸铁磨球硬度与内应力成正比,常因内应力过大造成零件失效。
Under traditional technique conditions, it is direct proportion that hardness to internal stress, because of inside stress overload, high-Cr grinding ball is failed.
成分设计对减少和改善内应力及其分布具有较大作用,它可促使磨球改性处理得到更佳效果。
Composition design play important action to improve inside stress and spread state of grinding balls, and obtains much more better effect.
分析和指明了PC制品在注塑成型生产中各个方面降低制品内应力的工艺方法、特点及要求。
This paper analyses the process, characteristics and requirement of the lowering of the internal stress of the PC products in the moulding.
钢丝矫直的目的是最大限度地消除钢丝生产过程中由于变形或温度分布不均造成附加内应力。
The aim of steel wire straightening is to maximally eliminate steel wire's extra internal stress caused by uneven deformation or uneven temperature distribution in production.
成分设计对减少和改善内应力及其分布具有较大作用,它可促使磨球改性处理得到更佳效果。
Composition design can have great effect on reducing and improving the internal stress and its distribution, making it possible for grinding ball improvement treatment to achieve better effect.
由于这种钢化内应力是一种永久应力,随着产品运行时间的延伸,它不会产生内应力衰减现象。
As this toughened internal stress is a kind of permanent stress, it can not produce the internal stress attenuation with elongation of the product service time.
岩石的外应力敏感指数仅受敏感常数的影响,岩石的内应力指数受敏感常数和孔隙度的共同影响。
Sensitivity index of external stress is only affected by sensitivity constant, while index of internal stress is affected by both sensitivity constant and porosity.
岩石的外应力敏感指数仅受敏感常数的影响,岩石的内应力指数受敏感常数和孔隙度的共同影响。
Sensitivity index of external stress is only affected by sensitivity constant, while index of internal stress is affected by both sensitivity constant and porosity.
应用推荐